Moin,

no time limit for nitrogen filled in line.

Nitrogen is used to shield potentially reactive materials from contact with oxygen. its is un reactive and its almost a inert  / noble gas.

Cheers
MM

On Sat, Feb 12, 2011 at 10:37 AM, syed moinul hasan <mhsyed1@gmail.com> wrote:
dear experts/friends,
may i know how long we can keep nitrogen in pipline before commissioning,  say 2 to 4 months.
I am i right? pl correct, if i am wrong.
regards
 
Moin-Oman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...