A weld for a welded pipe or a weld for an attachement to the pipe should not be located within a distance of approximately 6 times the pipe wall nominal thickness or 2" whichever is greater,
Regards
Manpreet Singh
On Fri, 11 Feb 2011 09:08:43 , Krishnakumar M S <krishnakumarms01@yahoo.com> wrote
Hi
Regarding my previous mail for discussion about Minimum weld clearance betewwn PIPE weld and Branch connection, I want to the case for in ASME B31.3 (Process Piping)
Thanks and Regards
Krishnakumar
FEDO
Regarding my previous mail for discussion about Minimum weld clearance betewwn PIPE weld and Branch connection, I want to the case for in ASME B31.3 (Process Piping)
Thanks and Regards
Krishnakumar
FEDO
----- Forwarded Message ----
From: manpreet <manpreetsin88@rediffmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tue, 8 February, 2011 11:55:53 AM
Subject: Re: [MW:9775] Minimum weld clearance in PIPING
Dear Kumar,
If you don't specify the design code, there would be an endless discussion for this topic (this has happened before) so please specify the code.
Regards
Manpreet Singh
On Tue, 08 Feb 2011 08:51:10 +0530 Krishnakumar M S wrote
>
>
> --
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
From: manpreet <manpreetsin88@rediffmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tue, 8 February, 2011 11:55:53 AM
Subject: Re: [MW:9775] Minimum weld clearance in PIPING
Dear Kumar,
If you don't specify the design code, there would be an endless discussion for this topic (this has happened before) so please specify the code.
Regards
Manpreet Singh
On Tue, 08 Feb 2011 08:51:10 +0530 Krishnakumar M S wrote
>
>
Hi,
> Hello,
>
>
>
>I have a case where the edge of the CS pipe fitting (90 deg. Elbow) coincideswith the branch connection pipe's weld. Header size: 10" and Branch is 2". The fittingedge is supposed to be fillet welded onto the pipe.
>Is this permissible?
>Pls tell me the min. clearance between weld ( But weld & Socket weld)
Thanks
>
>Krishnakumar
FEDO
>
>
>
> --
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment