Re: [MW:9787] special requierment in NACE electrode

Viral,

Please specify whether it is for upstream(NACE MR0175) or for Refinery(NACE MR0103). Specify for which Base materials the welding need to be performed.

J.GERALD JAYAKUMAR 00919344954677  


--- On Tue, 2/8/11, viral talati <viraltalati.143@gmail.com> wrote:

> From: viral talati <viraltalati.143@gmail.com>
> Subject: [MW:9786] special requierment in NACE electrode
> To: materials-welding@googlegroups.com
> Date: Tuesday, February 8, 2011, 5:11 PM
> Dear Friends,
> Is there any special requierment for electrode used for
> NACE material welding.
>
> regards
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>



____________________________________________________________________________________
No need to miss a message. Get email on-the-go
with Yahoo! Mail for Mobile. Get started.
http://mobile.yahoo.com/mail

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...