Dear Pradip,
Kindly go through UW 5 (b) (2) & (3) for more clarifications on un assigned base materials.
(2) For materials not identifiable in accordance with UG-10, UG-11, UG-15, or UG-93, but identifiable as to
nominal chemical analysis and mechanical properties, S-Number under Section IX, QW/QB-422, or to a material
specification not permitted in this Division, satisfactory qualification of the welding procedure under Section IX
is considered as proof of weldable quality. For materials identified by S-Numbers, the provisions of Section IX,
QW/QB-422 may be followed for welding procedure qualification.
The welding procedure need only be qualified once for a given nominal chemical analysis and mechanical
properties or material specification not permitted in this Division.
nominal chemical analysis and mechanical properties, S-Number under Section IX, QW/QB-422, or to a material
specification not permitted in this Division, satisfactory qualification of the welding procedure under Section IX
is considered as proof of weldable quality. For materials identified by S-Numbers, the provisions of Section IX,
QW/QB-422 may be followed for welding procedure qualification.
The welding procedure need only be qualified once for a given nominal chemical analysis and mechanical
properties or material specification not permitted in this Division.
(3) Material which cannot be identified may be proved to be of weldable quality by preparing a butt-joint
test coupon from each piece of nonidentified material to be used. Guided bend test specimens made from the test
coupon shall pass the tests specified in QW-451 of Section IX.
arun
On Fri, Feb 4, 2011 at 2:33 PM, pradip kumar sil <pradipsil@gmail.com> wrote:
Can anybody tell me how can i make wps/welder qualification in non ASME material. ASME SEC IX is applicable.regardsSil--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
அருணாசலம்
கலைவாணி
சுதர்ஷனா
வருண்
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment