ASME Sec.IX - Position is not an Essential Variable for WPS. So 4G WPS can use for 3G welder qualification with all other EV for welders are met.(P.No.,F.No., etc.,)

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 2/2/11, muthu barathi <muthu_barathi@rediffmail.com> wrote:

From: muthu barathi <muthu_barathi@rediffmail.com>
Subject: Re: [MW:9678] Re: WPS is 4G.. Can i qualify welder in 3G?
To: materials-welding@googlegroups.com
Date: Wednesday, February 2, 2011, 2:58 PM

When ever you want an answer you have to say complete details then only
you will get the correct answer.

You have to mention what is the code your supporting PQR u can not
change the code of your PQR qualified. according to that u have to
confirm. Ok even as per section IX also you can not qualify the welder.






On Wed, 02 Feb 2011 12:59:06 +0530 wrote
>Dear All.








If the code is ASME SEC 9.

Can i?



On Feb 2, 12:01 am, Suresh wrote:

> Dear Srinivas ,

>

> I truly agreed with Mr.karthik comment .

>

> Regards

>

> Suresh

>

>

>

>

>

> On Wed, Feb 2, 2011 at 10:23 AM, jaya anil
wrote:

> > Dear Srinivas,

>

> > Welder can be qualified in 3G Position using ur 4G WPS, no issue in
that.

>

> > No need of Qualifying WPS in 3G further .

>

> > Regards

> > Anil

> > On Tue, Feb 1, 2011 at 4:27 PM, Srinivas Engr <

> > srinivas.gmsr...@gmail.com> wrote:

>

> >> Dear all.

>

> >> I have a qualified WPS in 4G.

> >> Can i qualify welders to 3G position as per 4G wps without WPS

> >> qualification?

> >> Pl advise me. Its urgent.

>

> >> Thanks

> >> Srinivas

>

> >> --

> >> To post to this group, send email to materials-
welding@googlegroups.com

> >> To unsubscribe from this group, send email to

> >> materials-welding+unsubscribe@googlegroups.com
welding%2Bunsubscr­ibe@googlegroups.com>

> >> For more options, visit this group's bolg at

> >>http://materials-welding.blogspot.com/

> >> The views expressed/exchnaged in this group are members personel
views and

> >> meant for educational purposes only, Users must take their own
decisions

> >> w.r.t. applicable code/standard/contract documents.

>

> > --

> > To post to this group, send email to materials-
welding@googlegroups.com

> > To unsubscribe from this group, send email to

> > materials-welding+unsubscribe@googlegroups.com
welding%2Bunsubscr­ibe@googlegroups.com>

> > For more options, visit this group's bolg at

> >http://materials-welding.blogspot.com/

> > The views expressed/exchnaged in this group are members personel
views and

> > meant for educational purposes only, Users must take their own
decisions

> > w.r.t. applicable code/standard/contract documents.

>

> --

> Thanks & Best Regards,

>

> Suresh

>

> Mobile No: 91-92 92 905 905- Hide quoted text -

>

> - Show quoted text -



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...