Wednesday, February 2, 2011

Re: [MW:9680] details of equivalent materials list

http://www.splav.kharkov.com/steelgrade/mat_start_eu.php?name_id=10#1

or

http://www.arcelormittal.com/fce/prd_web/new_web_details.pl?code=A30&langlist=EN



Equivalent grades of grade   S355J2 (1.0577)
USA
-
Germany
DIN,WNr
Japan
JIS
European old
EN
China
GB
Sweden
SS
A656
St52-3N
SS490YA
Fe510D2
S355J2G4
Q345D
2134-01


Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 2/2/11, bujji <chakri.cruise@gmail.com> wrote:

From: bujji <chakri.cruise@gmail.com>
Subject: [MW:9676] details of equivalent materials list
To: materials-welding@googlegroups.com
Date: Wednesday, February 2, 2011, 2:51 PM

Hi All,
         can anyone give me the details of equivalent materials list ?
 
For eg : S355k2+N is EH-36 (40 MM plates)
 
 
S355 J2 is equivalent to ----------- ??? (round bar dia  70 mm)
 
 
Regards,
chakri.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...