Re: [MW:9676] Re: WPS is 4G.. Can i qualify welder in 3G?

If ASME Sec.IX - Yes you can..bcos Sec.IX Change in position is not an Essential Variable for WPS.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 2/2/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

From: Srinivas Engr <srinivas.gmsrini@gmail.com>
Subject: [MW:9673] Re: WPS is 4G.. Can i qualify welder in 3G?
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, February 2, 2011, 2:15 PM

Dear All.

If the code is ASME SEC 9.
Can i?

On Feb 2, 12:01 am, Suresh <bobsures...@gmail.com> wrote:
> Dear Srinivas ,
>
> I truly  agreed with Mr.karthik comment .
>
> Regards
>
> Suresh
>
>
>
>
>
> On Wed, Feb 2, 2011 at 10:23 AM, jaya anil <nethalaa...@gmail.com> wrote:
> > Dear Srinivas,
>
> > Welder can be qualified in 3G Position using ur 4G WPS, no issue in that.
>
> > No need of Qualifying WPS in 3G further .
>
> > Regards
> > Anil
> >   On Tue, Feb 1, 2011 at 4:27 PM, Srinivas Engr <
> > srinivas.gmsr...@gmail.com> wrote:
>
> >> Dear all.
>
> >> I have a qualified WPS in 4G.
> >> Can i qualify welders to 3G position as per 4G wps without WPS
> >> qualification?
> >> Pl advise me. Its urgent.
>
> >> Thanks
> >> Srinivas
>
> >> --
> >> To post to this group, send email to materials-welding@googlegroups.com
> >> To unsubscribe from this group, send email to
> >> materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscr­ibe@googlegroups.com>
> >> For more options, visit this group's bolg at
> >>http://materials-welding.blogspot.com/
> >> The views expressed/exchnaged in this group are members personel views and
> >> meant for educational purposes only, Users must take their own decisions
> >> w.r.t. applicable code/standard/contract documents.
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscr­ibe@googlegroups.com>
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> Thanks  & Best Regards,
>
> Suresh
>
> Mobile No: 91-92 92 905 905- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...