Hi,

It + /-5 degree C or 2% whichever is less.


On Wed, 02 Feb 2011 10:59:52 +0530 wrote
>Hello good morning,



I need details of electrode oven calibration.



How much percentage of temeparature variotion is allowable for

electrode oven calibration



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...