Thanks for your time, also Can you throw some focus on "Why is it recommended with uphill progression"?

Regards
Manpreet Singh


On Tue, 01 Feb 2011 21:55:46 , "Robert" <fusiondood@gmail.com> wrote

Strain-based pipeline design assumes that the pipeline may experience significant plastic strain during installation or while in service.  In order to avoid localization of this plasticity within the weld deposit, which could result in plastic collapse, consumables are selected to achieve a so-called "overmatching" condition between the weld metal and the adjacent base metal.  This is intended to produce a more favorable distribution of plastic strain across the weld joint.

 

--Robert

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of manpreet
Sent: Tuesday, February 01, 2011 4:36 AM
To: materials-welding
Subject: [MW:9643] Consumable for High strain Pipeline welding

 

Dear All,

Can somebody define High strain Pipeline Welding and why does it require much higher strength consumable than the base metal strength? For welding API 5L X60, Root pass is welded with E9016G, also why does it require Uphill progression? please provide your valuable inputs.

Regards

Manpreet Singh


http://sigads.rediff.com/RealMedia/ads/adstream_nx.ads/www.rediffmail.com/signatureline.htm@Middle

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...