Wednesday, February 2, 2011

Re: [MW:9668] WPS is 4G.. Can i qualify welder in 3G?

Dear Srinivas ,
 
I truly  agreed with Mr.karthik comment .
 
Regards
 
Suresh

On Wed, Feb 2, 2011 at 10:23 AM, jaya anil <nethalaanil@gmail.com> wrote:
Dear Srinivas,
 
Welder can be qualified in 3G Position using ur 4G WPS, no issue in that.
 
No need of Qualifying WPS in 3G further .
 
Regards
Anil
On Tue, Feb 1, 2011 at 4:27 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear all.

I have a qualified WPS in 4G.
Can i qualify welders to 3G position as per 4G wps without WPS
qualification?
Pl advise me. Its urgent.

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...