Wednesday, February 2, 2011

Re: [MW:9668] test required for EBW WPS

If ASME follow as below.
QW-215 Electron Beam Welding and Laser Beam
Welding
QW-215.1 The WPS qualification test coupon shall be
prepared with the joint geometry duplicating that to be
used in production. If the production weld is to include a
lap-over (completing the weld by rewelding over the starting
area of the weld, as for a girth weld), such lap-over
shall be included in the WPS qualification test coupon.
QW-215.2 The mechanical testing requirements of
QW-451 shall apply.
QW-215.3 Essential variables shall be as specified in
tables QW-260 and QW-264 for the applicable welding
process.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 2/2/11, Welding Material <weldingmaterial76@gmail.com> wrote:

From: Welding Material <weldingmaterial76@gmail.com>
Subject: [MW:9665] test required for EBW WPS
To: materials-welding@googlegroups.com
Date: Wednesday, February 2, 2011, 11:53 AM

Dear All
 
any body can tell me about tests required to qualify WPS by EBW.
 
 
Thanks & regards
 
Krishna

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...