Tuesday, February 1, 2011

Re: [MW:9658] welding of inconel 600

Dear Mr. Praveen,
please find attached files for Inconel
600, this will you helps you.

Saamy

On 2/1/11, praveen nair <praveen_nair9894@yahoo.co.in> wrote:
> dear experts,
>
> could u give some data for welding of inconel 600
> plate thickness 12mm
> which electode should i use for smaw , gtaw
> and have to withstand up to 1300c temperature
>
> praveen nair
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...