Re: [MW:9656] SAW filler for SA516 Gr70

Dear,

Go ahead with EH 14 for SA 516 Gr.70 plate wih Flux- SFA 5.17 F7P5 EH14.

Regards,

Vineet


On Sat, Jan 15, 2011 at 12:14 AM, rinshad abdul rahman
<rinshad043@gmail.com> wrote:
> Dear all,
> Which is the suitable filler for SAW on SA 516 Gr70 (with PWHT) ?
> EM12K or EM14K
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...