RE: [MW:9618] PWHT Thickness range

If Impact test is required, what would be the range?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Tuesday, 1 February 2011 1:00 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:9616] PWHT Thickness range

 

Assuming your PWHT is just stress relieving and no impact required, the range will be 5-50mm

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: Tuesday, February 01, 2011 7:46 AM
To: materials-welding@googlegroups.com
Subject: [MW:9612] PWHT Thickness range

 

Hi There,

 

Welding Code: ASME IX

Construction Code: ASME B31.3

 

Question: On PQR, test coupon was 25WT pipe and subject to PWHT. What would be the thickness range on WPS as per code above.

 

 

Thanks in advance,

 

Larry Zarate


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...