I need to know what the technical condition of a cutting machine to cut stainless tube Ø10X1
Thanks



    saludos
    L.. Caballero (Cluj napoca RU)

***************************************************************************
DISCLAIMER: This e-mail contains information property of Manufactura Moderna de Metales, SA, some or all of which may be legally privileged. It is for the intended recipient only. If an addressing or transmission error has misdirected this e-mail, please notify the author by replying to this e-mail. If you are not the intended recipient you must not use, disclose, distribute, copy, print or rely on this e-mail.
***************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...