Monday, February 14, 2011

[MW:9855] electrode selection of WPS of SA 333 Gr 6 low temp piping, GTAW +SMAW

Dear Sirs,

Pl advise how can select the electrodes for SA 333 Gr 6 (P1 and G1) low temp pipe.

I want to prepare WPS / PQR and then also WPQ for our current project.

Have selected the thickness around 5.55 mm (2 “S 80 pipe) for preparing WPS.

 

We followed the process of root run by GTAW and then by SMAW.

 

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.