Friday, February 11, 2011

[MW:9821] SA 516 Gr.60 high in manganese-accept or reject

Dear all,
                  We have received MTC for SA 516 Gr.60 plate of 10mm thickness with manganese of 1.47%,the lab test also give the same.

is it acceptable as per SA 516 SPEC.

Please confirm shall we accept or reject the plates,we have procured more tonnes of materails & started fabrication?

what shall we do in this stage?

How to overcome this issue ,pls guide

krishna


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...