[MW:9791] Re: RT requirements for Tanks as per API 620?

If 85% jnt efficiency, then spot RT is required.

API 620 states in 5.26 Radiographic/Ultrasonic Examination 5.26.4.3
(a)
When parts of tanks do not require complete examination,
circumferential joints in cylindrical or conical surfaces need to be
prepared and examined for a distance of only 3 in. on each side of any
intersection with a longitudinal joint. All joints in a spherical,
torispherical, or ellipsoidal shape or in any other surface or double
curvature shall be considered longitudinal joints.

On Dec 29 2010, 6:27 am, Srinivas Engr <srinivas.gmsr...@gmail.com>
wrote:
> Dear All
>
> Could anybody pl clear wats the RT requirement for Tank with Shell
> thickness of 12mm as perAPI620?
> Where to refer & Wat is the requirement?
>
> Rgds
> Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...