[MW:9674] PQR Base metal thickness Qualification

Hi,

To qualify a base metal thickness for 15 to 19 mm for construction code as per ASME B31.3, is it possible to qualify with a pipe coupon 24" x sch-80 (30.96 mm machined to 30 mm) (Due to material availabilty).

As per construction code above 19 mm, PWHT is required. Since this PQR is being qualified for base metal thickness from 15 mm to 19 mm, No PWHT will be done.

Can u clarify plz, will it be correct to choose this material. Also, can we achieve Hardness less than 248 HV10.

--
Regards
Yoganandhan.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...