[MW:9673] Re: WPS is 4G.. Can i qualify welder in 3G?

Dear All.

If the code is ASME SEC 9.
Can i?

On Feb 2, 12:01 am, Suresh <bobsures...@gmail.com> wrote:
> Dear Srinivas ,
>
> I truly  agreed with Mr.karthik comment .
>
> Regards
>
> Suresh
>
>
>
>
>
> On Wed, Feb 2, 2011 at 10:23 AM, jaya anil <nethalaa...@gmail.com> wrote:
> > Dear Srinivas,
>
> > Welder can be qualified in 3G Position using ur 4G WPS, no issue in that.
>
> > No need of Qualifying WPS in 3G further .
>
> > Regards
> > Anil
> >   On Tue, Feb 1, 2011 at 4:27 PM, Srinivas Engr <
> > srinivas.gmsr...@gmail.com> wrote:
>
> >> Dear all.
>
> >> I have a qualified WPS in 4G.
> >> Can i qualify welders to 3G position as per 4G wps without WPS
> >> qualification?
> >> Pl advise me. Its urgent.
>
> >> Thanks
> >> Srinivas
>
> >> --
> >> To post to this group, send email to materials-welding@googlegroups.com
> >> To unsubscribe from this group, send email to
> >> materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscr­ibe@googlegroups.com>
> >> For more options, visit this group's bolg at
> >>http://materials-welding.blogspot.com/
> >> The views expressed/exchnaged in this group are members personel views and
> >> meant for educational purposes only, Users must take their own decisions
> >> w.r.t. applicable code/standard/contract documents.
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscr­ibe@googlegroups.com>
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> Thanks  & Best Regards,
>
> Suresh
>
> Mobile No: 91-92 92 905 905- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...