Skip to main content

[MW:9660] RE: 9650] inconel welding electrode

International Nickel Company (INCO) was the originator of welding electrodes with compositions now designated as ASME Section II, Part  C, SFA-5.11 ENiCrFe-3 {SMAW) and SFA-5.14 ENiCr-3 {GTAW/GMAW}.    The registered trademarked names for these are INCONEL Welding Electrode 182 and INCONEL Filler Metal 82 respectively.  Recognition of INCO’s development, trade mark, and, ultimately, common usage, can be seen in the assigned UNS numbers;  i.e.  W86182  and N06082.  F43 encompasses a number for filler metal compositions including  ENiCrFe-3 and ERNiCr-3 as you can see by reviewing ASME Sc IX, QW-432.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ilangkumaran Kumarasamy
Sent: Tuesday, February 01, 2011 5:46 AM
To: materials-welding@googlegroups.com
Subject: [MW:9650] inconel welding electrode

 

Dear experts,

 

                        I have used sec II part C, for selecting electrodes and filler wires with sec IX, F no etc,. There is separate para for nickel and nickel alloys in sec IX. Eg F no:43  Now what is this Inconel welding electrode 82/ 182? Is there any different name for some other materials?

 

Can somebody explain me?

 

Ilan

 

 

**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouges state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...