[MW:9653] Re: WPS is 4G.. Can i qualify welder in 3G?

CODE is AWS D1.1


On Feb 1, 3:13 pm, "muthu barathi" <muthu_bara...@rediffmail.com>
wrote:
> Hi .
> you have not mentioned any code under which code u want to qualify?  
>
> On Tue, 01 Feb 2011 16:36:44 +0530  wrote
>
> >Dear all.
>
> I have a qualified WPS in 4G.
>
> Can i qualify welders to 3G position as per 4G wps without WPS
>
> qualification?
>
> Pl advise me. Its urgent.
>
> Thanks
>
> Srinivas
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-
> welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg athttp://materials-
> welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
> Dear Sir,
>
> Thanking You,
>
> Honesty is the best Policy
>
> With Warm Regards,
>
> Muthu Barathi P
> Mobile No:00962788269821 (Jordan)
>           00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...