Dear All,

Can somebody define High strain Pipeline Welding and why does it require much higher strength consumable than the base metal strength? For welding API 5L X60, Root pass is welded with E9016G, also why does it require Uphill progression? please provide your valuable inputs.

Regards

Manpreet Singh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...