chemical properties and reply friend please.
X 65 YS 448 MPa TS 531 MPa El %23 Impact at 0deg 27 Joules
C - 0.22 Mn - 1.45 P - 0.025 S - 0.015 Ti - 0.06
On Fri, 07 Jan 2011 17:00:34 +0530 wrote
>Using for root Er-70S2 and for capping & fill up E-7018
On Fri, Jan 7, 2011 at 3:41 PM, muthu barathi
Dear Friends,
Please let me know the best suitable welding electrodes for welding
tubular piles of materials API 5 L Grade X 65- PSL 2. Pipe size 1200 /
900mm OD wall thickness 20 mm
1 SMAW process
2 SAW process
Please give your valuable inputs.
Thanking You.
Muthu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
--
MANISH YADAV
08890122779,7877056928
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment