Please refer Babu's question
Regards
Will the ASME fillet welder (Qualified welder) ,qualified to tack weld the groove joint in fitup ?
Regards
From: César Alexis Viteri Pérez <alexis_viteri@hotmail.com>
To: Material Welding <materials-welding@googlegroups.com>
Sent: Fri, January 21, 2011 2:20:23 PM
Subject: RE: [MW:9373] Will fillet welder qualified to tack the groove Joint
Hi,
Mr. Suresh is right, for B31.3 u have to do tacks with qualified welder, see para 3.28.5.1-c:
(c)
Tack welds at the root of the joint shall be madewith filler metal equivalent to that used in the root pass.
Tack welds shall be made by a qualified welder or welding
operator. Tack welds shall be fused with the root
pass weld, except that those which have cracked shall
be removed. Bridge tacks (above the weld) shall be
removed.Best Regards
Date: Fri, 21 Jan 2011 14:37:25 +0530
Subject: Re: [MW:9368] Will fillet welder qualified to tack the groove Joint
From: bobsuresh24@gmail.com
To: materials-welding@googlegroups.com
I think No ,
Tack weld shall be done by qualified welder .
Regards
Suresh
On Fri, Jan 21, 2011 at 1:45 PM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi allAny one share official interpretation for the below situation.Will the ASME fillet welder ,qualified to tack weld the groove joint in fitup ?Thanks & Regards,K. Babu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Best Regards,
Suresh
Mobile No: 91-92 92 905 905
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments