Both Throat & Fillet were mentioned in drawings,
throat symbol=a ,
Fillet symbol=right angle triangle.
as per drawing you have to read the requirements.
throat symbol=a ,
Fillet symbol=right angle triangle.
as per drawing you have to read the requirements.
175, R.Kesavamoorthi,
Principal surveyor,
Quest (pvt.) Ltd.,
Ranipet.
From: krishnasamy masanam <krishnasamy1968@gmail.com>
To: materials-welding@googlegroups.com
Cc:
Sent: Thursday, 20 January 2011 8:10 PM
Subject: Re: [MW:9355] AWS Table 5.8 doubt???
Dear Friend!
Normally the fillet weld thickness is determined
by throat thickness, the design thickness calculated by least thick of
the base metal multiply by .0.7. and actual throat thickness
calculated by least length of the leg length multiply by 0.7 or
measured by Fillet gauge and cambridge gauge.
Have a nice day!
On 1/19/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
> Dear all,
>
> AS per AWS.I knw tat for fillet weld sizes we have to refer Table 5.8.
> My doubt is they given as weld size.
> weld size refer to throat or leg length? which one tat refers?
> clear me
>
> Thanks & Regards
> Srinivas
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To: materials-welding@googlegroups.com
Cc:
Sent: Thursday, 20 January 2011 8:10 PM
Subject: Re: [MW:9355] AWS Table 5.8 doubt???
Dear Friend!
Normally the fillet weld thickness is determined
by throat thickness, the design thickness calculated by least thick of
the base metal multiply by .0.7. and actual throat thickness
calculated by least length of the leg length multiply by 0.7 or
measured by Fillet gauge and cambridge gauge.
Have a nice day!
On 1/19/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
> Dear all,
>
> AS per AWS.I knw tat for fillet weld sizes we have to refer Table 5.8.
> My doubt is they given as weld size.
> weld size refer to throat or leg length? which one tat refers?
> clear me
>
> Thanks & Regards
> Srinivas
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment