Ramesh,
Please find the attached may benifit you.
regards,
Arun S Das
Inspection Engineer
Velosi Certification LLC
Qatar
Mob: +97433240549
+919847051202 ( India )
From: PRAMODH NAIR <pramodhnairmr@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Wed, 19 January, 2011 12:42:00 PM
Subject: Re: [MW:9322] Bolt Torque Value
Hi,
Find below attachment table for torque values for different rating of flange. Hope it will fullfill your requirement.
Flange Size | Insulated Set Torquing Values @0.15 | Standard Torquing Values | ||||||||||
F l a n g e R a t i n g | ||||||||||||
150 | 300 | 600 | 900 | 1500 | 2500 | 150 | 300 | 600 | 900 | 1500 | ||
1/2 | 35 | 35 | 35 | 120 | 120 | 120 | 29 | 46 | ||||
3/4 | 35 | 68 | 68 | 120 | 120 | 120 | 35 | 91 | 91 | 179 | ||
1 | 35 | 68 | 68 | 192 | 192 | 192 | 40 | 91 | 91 | 287 | ||
1 1/4 | 35 | 68 | 68 | 192 | 192 | 285 | ||||||
1 1/2 | 35 | 120 | 120 | 285 | 285 | 417 | 52 | 140 / 160 | 179 | 475 | ||
2 | 68 | 68 | 68 | 192 | 192 | 285 | 91 | 91 | 113 | 255 | 319 | |
2 1/2 | 68 | 120 | 120 | 285 | 285 | 417 | ||||||
3 | 68 | 120 | 120 | 192 | 417 | 585 | 113 | 160 | 179 | 319 | ||
4 | 68 | 120 | 192 | 285 | 585 | 1042 | 102 | 179 | 319 | 626 | ||
5 | 120 | 120 | 285 | 192 | 1042 | 1689 | ||||||
6 | 120 | 120 | 285 | 417 | 792 | 2565 | 179 | 428 | 695 | |||
8 | 120 | 192 | 417 | 585 | 1340 | 2565 | 199 | 287 | 695 | 1188 | ||
10 | 192 | 285 | 585 | 417 | 2099 | 5110 | 255 | 877 | 1188 | |||
12 | 192 | 417 | 185 | 792 | 2565 | N/A | 287 | 1320 | ||||
14 | 285 | 417 | 792 | 792 | 3692 | N/A | 428 | 1188 | 1563 | |||
16 | 285 | 585 | 1042 | 792 | 5110 | N/A | 380 | 1563 | 2233 | |||
18 | 417 | 585 | 1340 | 1042 | N/A | N/A | 558 | |||||
20 | 417 | 585 | 1340 | 1340 | N/A | N/A | 2010 | 3195 | ||||
24 | 585 | 585 | 2099 | 2099 | N/A | N/A | 3149 / 2354 | 5713 | ||||
26 | 585 | 1340 | 2099 | 2565 | N/A | N/A | ||||||
28 | 585 | 1340 | 2565 | 5110 | N/A | N/A | ||||||
30 | 585 | 1689 | 2565 | N/A | N/A | N/A | 780 | |||||
32 | 1042 | 2099 | 3692 | N/A | N/A | N/A | Conversion Factors | |||||
34 | 1042 | 2099 | 3692 | N/A | N/A | N/A | To Convert | Into | Multiply By | |||
36 | 1042 | 2565 | 5110 | N/A | N/A | N/A | LBFT (Torque) | Nm (Torque) | 1.3558 | |||
38 | 1042 | 1042 | 3692 | N/A | N/A | N/A | LBF / IN2 (Stress) | S/mm2 (Stress) | 0.008895 | |||
40 | 1042 | 1340 | 3692 | N/A | N/A | N/A | LBFT (Torque) | Kgm (Torque) | 0.1383 | |||
42 | 1042 | 1340 | 5110 | N/A | N/A | N/A | BAR (Pressure) | PSI (Pressure) | 14.5038 | |||
44 | 1042 | 1689 | 5110 | N/A | N/A | N/A | LBF (Load) | Newtons (Loads) | 4.448 | |||
46 | 1042 | 2099 | 5110 | N/A | N/A | N/A | % STRAIN / STRESS Conversion | |||||
48 | 1042 | 2099 | N/A | N/A | N/A | N/A | 0.10% | 30000 lbf/in2 | ||||
50 | 1689 | 2565 | N/A | N/A | N/A | N/A | 0.15% | 45000 lbf/in2 | ||||
52 | 1689 | 2565 | N/A | N/A | N/A | N/A | 0.20% | 60000 lbf/in2 | ||||
54 | 1689 | 3692 | N/A | N/A | N/A | N/A | Hydratight Max. Stress Recommendations | |||||
56 | 1689 | 3692 | N/A | N/A | N/A | N/A | Carbon Steels | 85% of S.M.Y.S. | ||||
58 | 1689 | 3692 | N/A | N/A | N/A | N/A | Stainless Steels | 65% of S.M.Y.S. | ||||
60 | 1689 | 3692 | N/A | N/A | N/A | N/A | Cupronickels | 70% of S.M.Y.S. | ||||
Duplex | 65% of S.M.Y.S. |
Have a nice day through out the year 2011.
Pramodh
From: alam <alampravez@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, January 18, 2011 2:36:07 PM
Subject: Re: [MW:9310] Bolt Torque Value
Hello Dear,
please find the details, if yuo need code wise i will provide you later.
Thank you
pravez alam
***********************************************************************************
Nom. Fig.Size Bolting No. Rec. Bolt Torque Torque Torque
Ins. (mm) x Dia. Ins Stress (lb/in2) 50% (Nm) 80% (Nm) 100%(Nm)
½ (15) 4 x ½" UNC 40,000 29 46 58
¾. (20) 4 x ½" UNC 40,000 29 46 58
1 (25) 4 x ½" UNC 40,000 29 46 58
1 ½ (40) 4 x ½" UNC 40,000 29 46 58
2 (50) 4 x 5/8" UNC 40,000 58 92 115
3 (80) 4 x 5/8" UNC 40,000 58 92 115
4 (100) 8 x 5/8" UNC 40,000 58 92 115
6 (150) 8 x ¾" UNC 40,000 103 164 205
8 (200) 8 x ¾" UNC 40,000 103 164 205
10 (250) 12 x 7/8" UNC 40,000 164 262 328
12 (300) 12 x 7/8" UNC 40,000 164 262 328
14 (350) 12 x 1" UN8 40,000 246 394 492
16 (400) 16 x 1" UN8 40,000 246 394 492
18 (450) 16 x1 1/8"UN8 40,000 286 457 571
20 (500) 20 x1 1/8"UN8 40,000 286 457 571
24 (600) 20 x 1 ¼" UN8 40,000 400 640 800
30 (750) 28 x 1 ¼" UN8 40,000 400 640 800
36 (900) 32 x 1 ½" UN8 40,000 708 1133 1416
On 1/18/11, Ramesh Barot <rameshnbarot@yahoo.com> wrote:
> Dear All Experts,
>
> Pl. tell me what is the torque value required for A325 property class 8.8
> M24
> bolt tightening?
>
> What wil be the max. value for it?
>
> Pl. give code reference.
> Thanks,
> With Best Regards,
> Ramesh Barot
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
Pravez Alam
Doha Qatar
Mob#+9746813248
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment