Re: [MW:9286] D1.1 Welder qualification Base metal

Hi,
refer AWS D 1.1 - Table 4.11 -

Table 4.11

Welder and Welding Operator Qualification—Number and Type of Specimens and Range of

Thickness and Diameter Qualified (Dimensions in Inches) (see 4.18.2.1)

and Table 4.10 for position limits.

Table 4.10

Welder and Welding Operator Qualification—Production Welding Positions Qualified by Plate, Pipe, and Box Tube Tests (see 4.18.1)

 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 1/17/11, Adi <adinraos@gmail.com> wrote:

From: Adi <adinraos@gmail.com>
Subject: [MW:9273] D1.1 Welder qualification Base metal
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Monday, January 17, 2011, 9:57 PM

Deal all

Please give me the code reference for Welder Base metal qualification
limitations in AWS D1.1


Adi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...