Mr Larry,
            Dr Leeb's hardness method is very unique one and usually conversions are not available. The only option is take the material perform Leeb Hardness and surrounding that point take 5 hardness readings in the required scale. Once you have the equivalent, now perform the Leeb hardness on the actual spot of the same material.

2011/1/17 Larry <quality@unieng.com.au>

 

Hi There,

 

Can anyone have an idea on how to convert Leeb Hardness Value HL to HV or HRC? Or anyone have a chart?

 

 

Many Thanks,

 

Larry Zarate

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...