Monday, January 17, 2011

Re: [MW:9252] WQT for Duplex SS

Hi Sujay,
As per sec.IX, SS welder is Qualified to weld the SDSS, nut you check with the client spec. also, bcz they will restrict this one.

Regards,

Mani.

On Sun, Jan 16, 2011 at 2:46 PM, PBR <pbrerode@gmail.com> wrote:
Dear Sujay,
          As per to the base metal grouping (ASME SEC IX QW-423.1),F number grouping (QW-432) no changes and so no need of separate qualification, but check other essential variables regarding welder performance refer QW-416.
 
With Regards,
P.Balajirajan.
 
 
-------Original Message-------
 
Date: 1/16/2011 12:59:37 PM
Subject: [MW:9239] WQT for Duplex SS
 
Dear All,
 
 Welder is qualified in SS material,it required separately  to be qualified for Duplex SS material.
 
thanks and regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
FREE winter Photo Animations for your email – by IncrediMail

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Regards,

E.Subramanian


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...