Skip to main content

RE: [MW:9138] Re: WPS and PQR for P 1 material and P 5

Dear Friends !
                        Greetings and thanks for your kindly information... my case the manufacturer recommend the Electrode E 9018 for capping, but material is IS 2062... that's way I have confused with this matter... I don't have WPSand PQR for this work... we have WPS & PQR for SA 106 Gr B and SA 335... but we can't use these WPS for above mentioned work?

       


Thanks & Best regards

 

Krishnasamy. M

Welding Inspector

Fize Al- Shammary Gen. Cont. Est.

Kingdom of Saudi Arabia.

Mob: +966 592823768




 
> Date: Thu, 6 Jan 2011 20:33:05 -0800
> Subject: [MW:9121] Re: WPS and PQR for P 1 material and P 5
> From: hindu.vikas@gmail.com
> To: materials-welding@googlegroups.com
>
> Dear Krishna,
> P-NO ,1, And material is is 2062 , so you done
> the root with E7018 OF 2.4mm, Welding Electrode and final caping with
> also same , but you have choice to done the final caping with 3.5mm
> welding rod, no need of E9018
>
>
>
> On Jan 5, 4:46 pm, "manpreet " <manpreetsi...@rediffmail.com> wrote:
> > Dear Krishna,Please explain your query in detail,if you are qualifying PQR then you can always choose different filler metals for different passes or&nbsp;If you&nbsp;have WPS which mention different filler metal for Cap, Also the title is vague&nbsp;"WPS and PQR for P 1 material and P 5", Please clarify.RegardsManpreet SinghOn Wed, 05 Jan 2011 16:59:32 +0530 Saamy wrote&gt;Dear All !&gt; Could you help me any one... We have IS 2062 material&gt;for rail welding... the manufacturer recommend for E 7018 for root,&gt;hot and filling and E9018 for capping on IS 2062... My Question is how&gt;to allow E 9018 on IS 2062? Both electrodes have different A No...&gt;That is essential variable... So please give advice...&gt;&gt;-- &gt;To post to this group, send email to materials-welding@googlegroups.com&gt;To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com&gt;For more options, visit this group's bolg athttp://materials-welding.blogspot.com/>Theviews expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.&gt;
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...