Dear Vinit

The MIG wire you are referring is a composite cored wire.

Please refer ASME Sec II Part C, SFA 5.9 wherein you will get all the tests to be conducted for batch qualification.

Regards

Prem Nautiyal


On Wed, 05 Jan 2011 14:33:47 +0530 wrote
>Dear all,

we want to take batch test qualification for EC 308LMIG welding(1.2MM DIA) .Can we know which tests will be applicable for this? also please send all lthe details( such as thickness of base metal ).We also want to carry out impact @-196C for this .Please share information regarding this.

Regards
Vinit




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...