Wednesday, January 5, 2011

Re: [MW:9099] Welder qualification Position range doubt? 4G doubt qualifies for?

As per ASME Sec IX : QW 461.9, if a welder is qualified in 4G on plate(groove), he gets qualified as follows:
(i) On Plate & Pipe( >24 in OD, groove weld) : Flat(1G) and Overhead(4G)
(ii) On Pipe( <=24 in OD, groove weld) : Flat(1G) for pipe OD > 23/8 in.
(iii) On Plate & Pipe( fillet weld) : Flat(1G), Horizontal(2G) and Overhead(4G).
 
please feel free to correct me if I am wrong.
On Wed, Jan 5, 2011 at 1:33 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All

If one welder qualifies in 4G...
As of practical he qualifies to all structural position tat 3g, 2G.

as per AWS D1.1, he only qualifies for 4G only - overhead.

pl clear me.. That if welder qualify to weld all position? or is he
only qualify for overhead?

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arnab Bakshi
Welding Engineer,
APIL Durgapur

(Alumnus)Dept. of Metallurgical and Materials Engg
NIT Durgapur

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...