Skip to main content

Re: [MW:9079] Re: Repair of Body cracks for A 217 Gr WC6

Suggest to follow ASME FFS-1/API 579-1 for detail assessement...
 
In my personal opinion, there will be high risk to repair valve for the said application...
 
Kind regards,
Panomsit

2011/1/3 Muni Andy <cmkfc07@gmail.com>
Dear Mr.Marcelo P. Soriano,
Thanks for your mail.
I understaood the situation.I am not telling to use as it is..
Take more care.Do repair.Pls ensure that the defect is removed.
Then you can use.
Getting new valve will take months.Also will cost more money.
Everyone cannot do the repair and it is not a easy task.but it is possible.
.Some expert guidance required.
C.Muniyandi
On 1/3/11, Marcelo P. Soriano Qa/Qc Eng'r.
<marcelopsoriano_1925@yahoo.com.ph> wrote:
> dear C.Muniyandi,
>
> Please considered the type of deffect as said by mister vinod that is
> (MULTIPLE CRACK) and also consider the type of service and pressure,
> specially the SAFETY and involvement of PROPERTY..
>
>  Material A 217 Gr WC6 , size 2 " X  2500 RTJ, H2 service
>
> thanks,
> marcelo p soriano
> technip qc eng'r
>
> On Jan 3, 12:56 pm, Muni Andy <cmkf...@gmail.com> wrote:
>> Dear Marcelo Soriano,
>> ASTM A217 permits repair welding.
>> We can do repair with approved welding Procedure and qualified welder.
>> Regards,
>> C.Muniyandi
>> Surveyor
>> Coimbatore
>>
>> On Mon, Jan 3, 2011 at 1:50 PM, Marcelo P. Soriano Qa/Qc Eng'r. <
>>
>>
>>
>> marcelopsoriano_1...@yahoo.com.ph> wrote:
>> > dear members,
>>
>> > in my opinion and experience theres bo any code telling that repairing
>> > welding of valve body* (casting) because in casting if you have crack
>> > on it and apply heat it will be larger and more cracks will run
>> > through the body, its better to replace it that than compromise the
>> > safety and property.....
>>
>> > thanks,
>> > marcelo soriano
>> > Technip Qc Eng'r
>>
>> > On Jan 2, 7:27 am, Vinod Jotwani <pooj...@yahoo.com> wrote:
>> > > Dear All,
>>
>> > > We have noticed multiple crack during the replica check in the control
>> > valve body ( Material A 217 Gr WC6 , size 2 " X 2500 RTJ, H2 service)
>> > during
>> > the fire incident at our Hydrocracker plant.  We would like to carry out
>> > the
>> > repair jobs for the same,
>>
>> > > Kindly share your experience and also advise whether advisable or not.
>> > Also share the WPS and cautions to be followed if repair performed by
>> > anyone
>> > in the group.
>>
>> > > Vinod
>>
>> > --
>> > To post to this group, send email to materials-welding@googlegroups.com
>> > To unsubscribe from this group, send email to
>> > materials-welding+unsubscribe@googlegroups.com<materials-welding%2Bunsubscr­ibe@googlegroups.com>
>> > For more options, visit this group's bolg at
>> >http://materials-welding.blogspot.com/
>> > The views expressed/exchnaged in this group are members personel views
>> > and
>> > meant for educational purposes only, Users must take their own decisions
>> > w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>>
>> - Show quoted text -
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...