Dear All,
 
Acording to our spec " Impact test sets shall be taken from 12 o'clock, 3 o'clock and 6 o' clock at
centre of weld
fusion line
+2mm from fusion line in the parent metal
 
Each test set shall include 3 specimens"
 
 
I have a doub't that we have to take the specimens  ex:   for centre of the weld 3specimens need to take at 12 o' clock  or 1 from 12,3and 6o'clock respectivly
 


--
 

Best Regards,

K.V.S.Reddy,
Q.C.Inspector(Piping&Welding),
BS-132 Project,
SKEC Eng& Con Ltd.,
Postbox no-55653,
Sabahiya-54567,
Kuwait.
kvsreddy777@gmail.com,karryswamireddy@yahoo.com,
Ph:00965-94414396.
PleaseSave a tree. Don't print this e-mail unless it's really necessary

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...