[MW:9479] Re: P12 Vs P22 qualification

if it is for PQR,  you require new qualification, however for performance yes, you can provided other variables are similar (QW 423)

On Wed, Jan 26, 2011 at 12:43 PM, dinesh patil <dinn_1981@rediffmail.com> wrote:
sir ,

       i have some problem sir P12(GTAW) qualified welding can weld the P22 joint(GTAW).pl Explain me i m so confuse

Regards

Dinesh S Patil

09662844808




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...