Dear All
the weld between of a pressure vessel with a support that must be qualified according AWS D1.1OR ASME VIII?
REGARDS
E71T-1C is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...