Dear All,
PQR "1434" with P1 Gr2 materials with 12.7mm base metal thickness,
A repair PQR "1458" prepared with same materials for same 12.7mm base metal thickness, repair WPS "5799-10" for PQR 1458 have base metal thickness of 9.5mm,
since Impact test is mandatory, base metal thickness limits shall be 12.7 to 25.4mm, which means WPS is not qualified, Please confirm my understanding.
Regards
Manpreet Singh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
PQR "1434" with P1 Gr2 materials with 12.7mm base metal thickness,
A repair PQR "1458" prepared with same materials for same 12.7mm base metal thickness, repair WPS "5799-10" for PQR 1458 have base metal thickness of 9.5mm,
since Impact test is mandatory, base metal thickness limits shall be 12.7 to 25.4mm, which means WPS is not qualified, Please confirm my understanding.
Regards
Manpreet Singh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.