Dear All
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Which one of the penetrameter is more stringent DIN 10/16 or DIN 6/12? Actually as per the requirement DIN 6/12 should have been used for 6'' SCH 160 carbon steel pipe but they have used DIN Fe 10/16. I think it should be acceptable if the DIN 10/16 is used for thinner materials than 6'' SCH 160 carbon steel. A table in this regard would be helpful.
best regards
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments