Dear All,
Can anybody describe what is "Certificate of conformance"?
We have got all the project related documents from Vendor, Can you detail, what all submissions are required other than Project Documents, I have listed some of them as:-
*As-Built Drawing
* MRB
* Certificate of compliance
Please provide your inputs if there is something else required?
Best Regards
Manpreet Singh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.
Hello, Please see the response below. Regards. P. Goswami, P. Eng, IWE. From: materials-welding@googlegroups.com <materials-weld...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...