[MW:9184] Re: RELATION BETWEEN WPS & WPQ THICKNESS LIMITS.

Yes, you can qualify, QW403.6, impact thickness limits will not apply
to WPQ (performance qualification)
Case 1: WPS T limits 7.11-14.22
Case 2: WPS T limits 1.7-6.8

however for WPQ, limits will be 1.5 to 2t in both the cases (QW404.30)

On Jan 11, 7:56 pm, Venkat Ramulu <cvram...@yahoo.com> wrote:
> Dear All,
> Any body can clarify,
>
> 1)We have established WPS & PQR for P8 matirial,7.11 thick with  -196ºC
> impact.Based on this WPS, shall I qulify WPQ with 5mm  thick ?. If yes what will
> be the range of qualification.
> 2) Other WPS & PQR for P8&3.4 thik with  -196ºC impact. Based on this if  a WPQ
> is qualifide with 5mm thick,what would be the thickne range of qualification? Is
> it 1.7 to 6.8 or 2.5 to 10mm? give code reference.
> 3) Is there any relation between procedure & performance qualification thickness
> limits.Give me code reference.
>
> Regards,
> C.Venkatramulu.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...