Tuesday, January 11, 2011

[MW:9170] Fw: API 530 Sollution annealing after coiling of SA213 TP304H

Dear All,
Further to my below quirey,i will add up some more points which relate to that.
 
Material: SA213 TP304H- Tube-Dia-101.6x8.55mm.thk.
Design Code-API530
Construction code : Sec.VIII,Div.1/B31.3
Inside bending radius - 1750mm
OD - 3500mm
Design temp - 300 degree celsius
 
According to UHA44 or B31.3,need postfabrication heattreatment or not?

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 1/11/11, Karthik <karthik6684@yahoo.com> wrote:

From: Karthik <karthik6684@yahoo.com>
Subject: API 530 Sollution annealing after coiling of SA213 TP304H
To: materials-welding@googlegroups.com
Date: Tuesday, January 11, 2011, 9:22 AM

Dear All,
Please give your views on below quirey.
Material: SA213 TP304H- Tube-Dia-101.6x8.55mm
Code: API530.
The above material has sollution annealed at 1040 degree celsius from material manufacturer.We are going to make coiling of these tubes(Coil Dia-3.5Mx8M(height) ).
Quirey:
01. Does sollution annealing to be done again after coiling of these tubes? because our customer asked us to do Sollution annealing after coiling.(they referred to ASME Sec.II-Part-A)Also our customer not aware of API530 requirements.Also I dont have API530 book.
 
02.Please give, is there is any requirement as per API530?

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...