As I understand about MR-0175, hardness requirement is only one of the requirements for NACE -0175.To meet NACE 0175 requirements any material has to undergo a series of evaluations so as to justify and meet the design and service requirements in H2S containing environments in oil and gas production.It supplements, but does not replace, the material requirements given in the appropriate design codes, standards or regulations
 
MR0175/ISO 15156 describes general principles, requirements and recommendations for the selection and qualification of metallic materials for service in equipment used in oil and gas production and in natural gas sweetening plants in H2S-containing environments.It addresses all mechanisms of cracking that can be caused by H2S, such as sulfide stress cracking, stress corrosion cracking, hydrogen-induced cracking and stepwise cracking, stress-oriented hydrogen induced cracking, soft zone cracking and galvanically induced hydrogen stress cracking. For all the above cracking to happen BM/WM/HAZ hardness is a very important  factor. Hardness depends a lot of factor, chemical composition,  type of processing and related thermal properties, subsequent heat treatment and others. Hence just by through controlling hardness an alloy does not qualify for NACE MR-0175.
 
Basically any material conforming to NACE MR 0175 has to meet a list of requirements specified by the designer and the requirements have to be met by the manufacturing mill or the suppliers.This applies to any finished product and may apply to welding consumables also.
 
Before selecting or qualifying materials using other parts of NACE MR0175/ISO 15156, the user of the equipment shall define, evaluate and document the service conditions to which materials may be exposed for each application. The defined conditions shall include both intended exposures and unintended exposures which may result from the failure of primary containment or protection methods. Particular attention shall be paid to the quantification of those factors known to affect the susceptibility of materials to cracking caused by H2S.

Factors, other than material properties, known to affect the susceptibility of metallic materials to cracking in H2S service include: H2S partial pressure, in situ pH, the concentration of dissolved chloride or other halide, the presence of elemental sulfur or other oxidant, temperature, galvanic effects, mechanical stress, and time of exposure to contact with a liquid water phase

Materials for NACE environments may be pre-qualified -based on documented service experiences and through laboratory testing.

The above is a general guideline on Material requirements for MR.-0175.If you have any specific problem, query, feel free to ask.

Regarding the other query:- Why does weldable stainless steels (i.e. 316L) contain less carbon than standard grade stainless steels?- TO IMPROVE CORROSION RESISTANCE, ESPECIALLY TO  IMPROVE INTERGRANULAR CORROSION RESISTANCE AND STRESS CORROSION CRACKING RESISTANCE IN SOME MEDIAS, THROUGH CONTROL OF HARDNESS.
 
Hope this will clarify your query.
 
Thanks
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
 


From: Idris Mohiuddin [mailto:idrismohi@gmail.com]
Sent: Sunday, January 09, 2011 6:44 AM
To: pgoswami@sympatico.ca; pgoswami@quickclic.net
Subject: Requirement of NACE MR0175 / SS

Dear sir,
 
Sorry for mailing you on your personal email, but I didnot received any response for this query posted on material & Welding blog.
 
So please answer me for the below mentioned query's:

Please specify In addition to hardness testing, what is the other main requirement in NACE MR0175?
Why does weldable stainless steels (i.e. 316L) contain less carbon than standard grade stainless steels?
 
Thanks in advance

Regards,
 
MIM
Inspection Engineer
FAHSS / TUV
KSA

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...