Monday, January 3, 2011

[MW:9070] E71T1-G

Hi members,
1. Above mentioned electrode is given in our WPS for offshore pipe line welding for FCAW process but i could not find its chamical composition.Can i use this electrode? if yes, pls tell me the reference.
2. Is preheat necessary while thk is 14.28mm?


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.