Re: Re: Re: [MW:8838] Difference between E-7016 & E-7018


HI
please refer ASME sec II part C FOR CONSUMABLES U MAY REFER ELECTRODE CLASSIFICATION AND REFER THE MANUFACTURER'S RECOMMENDATION




E70 16 HERE 1 DENOTES ALL POSITION WELD AND IT IS A LOW HYDROGEN SO BETTER GO FOR REDRY TO REDUCE HYDROGEN INDUCED CRACK
On Sun, 19 Dec 2010 22:07:51 +0530 wrote
>
>

>
Hi,
>

>
Both electrodes you may use and both require baking both are suitable
>
for all position and E7016 is costlier than E7018 and more over E7018
>
will give approximately about 15 / 20% volume of weld metal than E7016
>
as E 7018 has iron powder is mixed in its flux.
>

>

>

>
On Sun, 19 Dec 2010 12:34:06 +0530 wrote
>
>E 7018 is all position electrode requiring baking/ heating for sound
>
weld. E7016 is flat position welding electrode and does not require
>
baking/ heating for sound weld.
>

>
Pramod Tiwari
>

>

>
On Sat, 18 Dec 2010 17:44:52 +0530 pradip kumar sil wrote
>

>
>Dear sir,What is the quality wise difference between E-7018 ( BASIC
>
LOW HYDROGEN)& E-7016 ( BASIC SODIUM LOW HYDROGEN).Can i use E-7018
>
insted of E-7016.Where is the specific area of these two
>
electroderegardssil--
>

>
>To post to this group, send email to materials-
>
welding@googlegroups.com
>

>
>To unsubscribe from this group, send email to materials-
>
welding+unsubscribe@googlegroups.com
>

>
>For more options, visit this group's bolg at http://materials-
>
welding.blogspot.com/
>

>
>The views expressed/exchnaged in this group are members personel views
>
and meant for educational purposes only, Users must take their own
>
decisions w.r.t. applicable code/standard/contract documents.
>

>
>
>

>

>

>

>
--
>
>
>
To post to this group, send email to materials-welding@googlegroups.com
>
>
>
To unsubscribe from this group, send email to materials-
>
welding+unsubscribe@googlegroups.com
>
>
>
For more options, visit this group's bolg at http://materials-
>
welding.blogspot.com/
>
>
>
The views expressed/exchnaged in this group are members personel views
>
and meant for educational purposes only, Users must take their own
>
decisions w.r.t. applicable code/standard/contract documents.
>
>
>


Dear Sir,
>

>

>

>

>

>
Thanking You,
>

>
Honesty is the best Policy
>

>
With Warm Regards,
>

>
Muthu Barathi P
>
Mobile No:00962788269821 (Jordan)
>
00962775401951




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...