RE: Re: [MW:8704] Reg: AWS-CWE

Mr. Ayyappan,

 

You could also refer to TWI website from UK. They have some courses conducted in Chennai but slightly expensive.

 

Regards,

Ekalavya

Managing Director

Cimotec Hydro Machines Pvt. Ltd

Bangalore

mail@cimotecindia.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rakesh Pandey
Sent: Saturday, December 11, 2010 12:00 AM
To: materials-welding@googlegroups.com
Subject: Re: Re: [MW:8689] Reg: AWS-CWE

 

In India, a company called Quality Concept in Chennai provides course for AWS. You can get the contact by googling.

Regards,
Rakesh Pandey
Chevron Nigeria Limited

On Sat, 11 Dec 2010 10:54:55 +0530 wrote
>Dear Mr.Ayyappan
 
Can you give me guide were we can do IWE Dipolma
 
Priyamudan
NK.PALANIYAPPANWelding Inspector
Galfar Al Misnad Engg. & Contrg. WLLPost Box 22170
Doha, State of QatarMobile: +974-66876603
Mobil:  +91-9791409275Palaniyappan1983@gmail.com
palaniappan17728@galfarqatar.com.qaWeb: www.galfar.com & www.galfarqatar.com





On 10 December 2010 08:08, Ayyappan Subramanian wrote:






Dear All,
 
I'm Ayyappan from India.
I'm a post graduate Engineering degree holder in Welding Technology with 7 years of experiance in various fabrication Industry.
And also I'm certificate holder of IWE Diploma,API-510, AWS-CSWIP-CWI.
I would like to have some information regarding AWS-CWE(Certified welding Engineer)
Can any one provide the information regarding Eligibility criteria, Course Condutor In India, Fees Structure Etc!!!!
To my knowledge, there is some provision to attain the certificate without examination for the professional welding engineer degree holder along with IWE . But i could not find any aithentic information.

Can any one get me clarified .
 
With regards,
S.Ayyappan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


Regards,

Rakesh Pandey
Mob. +2348079199559

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...