Dear Vivek,

as everyone said like dust test is nothing to do with blasting
profile,it is just ensuring that the surface is ok for priming,one
more thing that you didnt mention the type of abrasive you are
using,if it is metallic abrasive dust test is not
required(SSPC)because recylable abrasive will not make dust after
hitting the substrate but expendable abrasive like copper slag will
shattered into small pieces after hitting,in this case it is a good
practice to do the dust test to ensure the quality

I hope it will help you, if anybody have any concern please let me
know

Thanks & Regards

Haseeb.P.H

On Dec 22, 12:50 pm, Vivek K <vivekk....@gmail.com> wrote:
> Dear All,
>
> If the blasting profile is to be SA 2 1/2, whether dust contamination test
> is mandatory on the blasted surface.
>
> Thanks and Regards
> K. Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...