Dear All,

 

Please refer to ASME Sec. IX edition 2010 in which no “S” number classification specified. All S number has been indicated with respective P number classification. In fact some of EN and JIS materials and ISO equivalent group number also specified.

 

Regards,

 

L. Prabhu kumar.

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sundaram Elumalai
Sent: Wednesday, December 22, 2010 9:43 AM
To: materials-welding@googlegroups.com
Cc: Yul Tagalog; Jaffar A Alfardan; Jamal Budeiri; Ala Saket
Subject: RE: [MW:8867] Welding between A106 Gr.B and API 5L Gr.B

 

No, API 5L  Gr.B is S1 group and will not cover the P1. So he has to qualify the PQR.

 

P1 covers S1 but S1 will not cover P1.    QW 420.2

 

 

 

 

With Kind regards,

 

S.Elumalai.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of SOHAIB GHNAIMAT
Sent: Tuesday, December 21, 2010 6:54 PM
To: materials-welding@googlegroups.com
Cc: Yul Tagalog; Jaffar A Alfardan; Jamal Budeiri; Ala Saket
Subject: Re: [MW:8859] Welding between A106 Gr.B and API 5L Gr.B

 

In accordance with ASME IX, (ASTM 106 Gr B) and (API 5L Gr B) have the same P-no and therefore , you don't need to qualify new WPS it covers BOTH.

 

Regards,

 

Sohaib

 

 


From: Elshan Feyzullayev <elshan_f@hotmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, December 21, 2010 2:14:06 PM
Subject: RE: [MW:8858] Welding between A106 Gr.B and API 5L Gr.B

in accordance ASME IX 2001 edition QW 420.2 you can use this WPS for welding of ASTM 106 Gr b to API 5L Gr B.
 
regards,
Elshan.


> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of thiru sam
> Sent: Tuesday, December 21, 2010 4:14 PM
> To: Materials & Welding
> Subject: [MW:8853] Welding between A106 Gr.B and API 5L Gr.B
>
> Dear All,
>
> One of my contractor submitted and wps/pqr for approval for welding
> between A106 Gr.B and API 5L Gr.B pipes.
>
> The Wps is prepared newly for this project and PQR is from old
> projects.
>
> I reviewed and i found that the PQR is done for API 5L PSL1-Gr.B to
> API 5L PSL1-Gr.B.
>
> Is it possible to prepare the wps for A106 Gr.B and API 5L Gr.B pipes
> based on the above PQR.
>
> Please reply.
>
> Thanks.
>
>
> Filtered by Hosted Filtering
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...