RE: [MW:8856] Reducing hardness of EN-24 material.

Dear Prinka,
                 1)You have any PQR for this?
                 2)If not call some good elotrode supplier they will suggest and supply electorde and help to make PQR.
Regards
Anant
  

Date: Mon, 20 Dec 2010 10:17:42 +0530
Subject: Re: [MW:8826] Reducing hardness of EN-24 material.
From: piyuwillseeu@gmail.com
To: materials-welding@googlegroups.com

Dear All,
 
Thank you for your valuable reply. I have taken a note of your answers.
 
The main reason to reduce the hardness of EN-24 flat is, I want to weld it at some locations. But the welding is getting cracked.
 
I have just taken a sample and done Normalising of it.
 
The hardness values before Normalising are: 249, 244 HBW.
 
The hardness values on the same points after Normalising are: 404, 415 HBW.
 
The main problem is to weld the EN-24 flat (40 X 16mm thk.) with SA 516 Gr. 70 plate (6mm thk.).
 
Please tell me the solution for the same.
 
Thanks & Regards,
 
Priyanka Deshmukh.

On Sun, Dec 19, 2010 at 5:48 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Please specify:
You intended to reduce hardness from what  to what values? On what basis?
Why did you choose Normalising, what exactly did you do?
What you needed was Annealing in principle. But still a lot needs to be put together...

--- On Sun, 19/12/10, Priya Deshmukh <piyuwillseeu@gmail.com> wrote:

From: Priya Deshmukh <piyuwillseeu@gmail.com>
Subject: [MW:8800] Reducing hardness of EN-24 material.
To: materials-welding@googlegroups.com
Date: Sunday, 19 December, 2010, 12:21 PM



Dear All,
 
I wanted to reduce the hardness of EN 24 material. For that I employed Normalising on the material.
 
But the hardness increased instead of reducing.
 
Can U please suggest me the reasons for this and how to reduce the hardness of the material.
 
Thanks & Regards,
 
Priyanka Deshmukh.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Priyanka Deshmukh,
Quality Control Engineer,
Transparent Energy Systems Pvt. Ltd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...