Sunday, December 19, 2010

Re: [MW:8808] Difference between E-7016 & E-7018

Both can be used, but deposition efficency in 7018 is more than 7016 due to iron powder
7016 is very familiar in japan as 7018 in india
kgp

On Sat, Dec 18, 2010 at 5:26 PM, pradip kumar sil <pradipsil@gmail.com> wrote:
Dear sir,
What is the quality wise difference between E-7018 ( BASIC LOW HYDROGEN) & E-7016 ( BASIC SODIUM LOW HYDROGEN).Can i use E-7018 insted of E-7016.
Where is the specific area of these two electrode
regards
sil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...